BELZONA® PROVIDES LONG-TERM PERFORMANCE IN BRIDGE JOINTS

KHIA ID: 4672
Industry: Buildings & Structures (BSTR)
Application: FPA-Floor Problem Areas (FPA)
Substrate: Concrete and steel
Customer Location: Department of Transportation, USA
Application Date: 2005
Products:

Belzona® 4521 (Magma-Flex Fluid)


Problem: Joints needed to be sealed between existing armor plates on the bridge
Photograph Descriptions
  1. Application of Belzona® 4521 between the armor plates
  2. The intentional pinhole in the bay beneath Belzona application remains unchanged after 5-year service
  3. The bays on the east end of the bridge beneath Belzona application shows no signs of leakage after 5-year service
Application Situation
Joints in the east embankment of the bridge
Application Method
Application was carried out in accordance with the Belzona Know-How System Leaflet FPA-6 using approximately 200 cu in of Belzona® 4521.
Belzona Facts
Belzona solution has a long successful history providing long term performance. After 5 years in service, Belzona® 4521 application was reviewed and showed no signs of leakage after several hours of hard rain. An intentional pinhole was added during installation to test failure resistance. Pinhole also remained unchanged after 5 years. A conventional silicone joint material installed on the other part of the bridge began leaking within 12 months of being placed.