Belzona Repairs Broken Dielectrics

KHIA ID: 542
Industry: Power (POWR)
Application: GSS-Gaskets, Seals and Shims (GSS)
Substrate: Porcelain
Customer Location: Power station - Egypt
Application Date: February 2005
Products:

Belzoana® 1111 (Super Metal)


Problem: Dielectrics were broken at their edges causing oil infiltration from the connecting transformer.
Photograph Descriptions
  1. The broken dielectrics
  2. Making a former on the good edge using Belzona® 1111
  3. Reforming the broken edge
  4. The two repaired dielectrics
Application Situation
Porcelain dielectrics (insulators)
Application Method
Application was carried out in accordance with a modified version of Belzona Know-How System Leaflet GSS-1.
Belzona Facts
Belzona solved a serious problem in the dielectrics. Instead of buying new units, saving more than $5,000. The dielectric strength of Belzona® 1111 made it a suitable choice for this application.